tombstoning (leadfree solder paste) | 15 July, 2004

WERW HAVING PROBLEM IN OUR PRODUCT SINCE WE STARTED USING A LEADFREE SOLDER PASTE..REJECTS OF TOMBSTONING IS SO ERRATIC...HOPE YOU CAN GIVE SOME INPUTS HOW TO CONTROL THIS..WHAT IS THE POSSIBLE CAUSE?THANKS

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#29515

tombstoning (leadfree solder paste) | 15 July, 2004

Get started by searching the fine SMTnet Archives. We love talking about tombstoning and solderballs. Good luck.