Standard for Solder Spread Test | 30 June, 2004

I get always a lot of evaluations including results from Solder Spread tests, but it seems everybody creats his own test methode. Is there a official Standard or test instruction for Solder Spread Testing such as IPC, MIL, DIN...

Thanks

Chris

reply »

#29339

Standard for Solder Spread Test | 1 July, 2004

For a quantatative measure of solder spread use: * IPC-S-804/805 * Mil-F-14256E,4.7.5