MOLE

#28694

MOLE | 20 May, 2004

I need some advice on how to run a test with some large boards through the re-flow oven. The boards are 17"x17", 3/16" thick. Withought destroying one of the boards, how would I go about getting a good temperature profile?

reply »

mrmaint

#28696

MOLE | 20 May, 2004

Doug, If you are worried about cooking the board. Take a know profile and either reduce the heat in each zone or increase the belt speed.This should keep you from cooking the board. then adjust the profilr to the board from there.

MrMaint

reply »

#28721

MOLE | 22 May, 2004

Try either: * Scrap board from the board fabricator * Large peice of blank FR4