Glue Bubbles

Marco Serrano

#27953

Glue Bubbles | 7 April, 2004

Had anyone experienced air bubbles inside of the Loctite glue syringes? If any of you do What have you done to rid off this problem? Thanks in advance!

reply »

Paul

#27954

Glue Bubbles | 7 April, 2004

The easiest way to remove air bubbles from any fluid is to place it into a vacuum chamber. I do this almost daily with liquid rubber coatings, glues, and plastics.

reply »

#27968

Glue Bubbles | 8 April, 2004

We typically store the tubes straight up and down. This seemed to help with the air pocket problem. Did not solve it 100 percent. best bet is still vacum.