BGA REBALL | 27 June, 2000

I need a reball kit for high temp balls. can anyone help?

Thanks Leon

reply »

Chris May

#3679

Re: BGA REBALL | 27 June, 2000

Leon,

Have you tried a piece of glass, deposit some flux onto glass, place the BGA in the glass to flux it, replace BGA and reflow using existing solder deposition ??

Regards,

Chris

reply »

Leon Lovell

#3680

Re: BGA REBALL | 27 June, 2000

Hello Chris Thanks for the reply. I have not tried that. How does that work? What I want to do is replace the Ball on a cbga. leon

reply »

KamranT

#3681

Re: BGA REBALL | 29 June, 2000

Try this .Solderquik.com for the balls and you could get Micro stencil from .Minimicrostencil.com This way you can paste and reflow.

reply »

Glenn Robertson

#3682

Re: BGA REBALL | 29 June, 2000

Leon -

Remember for a CBGA you will need to use high-temp solder balls. IBM can supply the recommended solder paste (eutectic) volume.

Glenn Robertson