Should I have any concerns with operators using flux for handsoldering, straight out of a 25 ltr drum which is not even thinned dowm to the correct SG level. The flux is Alpha 615-25 RMA based and we use it in our wavesoldering process.

Thanks in advance

Sam

reply »

Steven

#27312

Handsoldering/Rework Flux | 18 February, 2004

my experience tells me you should have no problem. However please remove the flux residues from the board. Unless of course this is a product that is inexpensive and you don't care about degradation/flux migration etc. In example an electronic toy. There are many fine flux removing aerosols on the market place take a look at Microcare.com.