Stick on robber/thief pads for wave soldering


Loz

#26925

Stick on robber/thief pads for wave soldering | 19 January, 2004

Wondering if anyone knows if this product actually exists? If so please provide details.

Thanks,

Loz

reply »

#26926

Stick on robber/thief pads for wave soldering | 19 January, 2004

Not as such. Choices are: 1 Cut and epoxy some board foil from your board fabricator. 2 Sacrifice part a pad repair kits from the likes of: * Engineering Lab 905-785-1982 * Circuit Technology Center 978-374-5000 * General assembly suppliers catalog house [ie, Contact East, Techni-Tool, etc]

reply »


RDR

#26932

Stick on robber/thief pads for wave soldering | 19 January, 2004

I once used some foil tape from 3M with hightemp adhesive. It actually sorta worked.

Russ

reply »