Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


SMT MCX connector

Phil

#26914

SMT MCX connector | 16 January, 2004

I have a connector which has very weak joints. Solder fractures easily. On inspection the solder is very grainy and full of voids. Process is 63/37 no clean. Any thoughts?

Phil

reply »

#26917

SMT MCX connector | 16 January, 2004

Doesn't sound good.

Is it only the connector that solders poorly? Tell us more about the solder, solder fracture, connector pins involved, and what not. Good any nice picture?

reply »

Custom Conformal Coating Masks

fluid dispensing pumps for integration