PCB bake-out after cleaning

blnorman

#26640

PCB bake-out after cleaning | 17 December, 2003

I may have asked this question before but couldn't find anything when I ran a search. Question, after ultrasonically cleaning our boards we bake them out to drive off residual moisture. Current requirement is 24 hours @ 105�C. I seem to remember a post that stated 4 - 8 hours @ 105� would be adequate. What say ye?

reply »

#26649

PCB bake-out after cleaning | 17 December, 2003

Francois Monette [Cogiscan Inc. 450-534-2644 fmonette@cogiscan.com ] is the resident genius on component and board baking. If he doesn't chime-in a in a day or so, give him a shout. He seems to nap quite a bit.

Alternately, if you search on his name, you'll probably find the posting that you're trying to recall.

reply »