Is this safe to wavesolder the PCB in wave contaning carbon pads for switch or somekind of masking is to be put on that pads.

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#24047

Wave soldering of Carbon Switch pads on PCB | 7 April, 2003

It depends on the carbon polymer that the fabricator printed on your board. It could be: * No wave soldering * Wave soldering with a peelable mask * Wave soldering

... probably one of the latter two. Watch it. Some temporary masks can affect the polymer.