ULTRASONIC WELDING

HAROLD LICHT

#23661

ULTRASONIC WELDING | 5 March, 2003

WE HAVE A NEED TO BOND SOME LOW TEMPERATURE LED'S TO A THIN CIRCUIT BOARD LAMINATED TO A HEAT SINK. HAS ANYONE USED AN ULTRASONIC WELDER TO WELD COPPER GUL WING LEADS TO A COPPER PAD USING ULTRASONICS? IF NOT HAS ANYONE USED RESISTANCE SPOT WELDING FOR COPPER TO COPPER? PLEASE RESPOND VIA E-MAIL TO HAROLD.LICHT@SIEMENS.COM

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @