I am currently exploring the option of screenprinting chipbonder for backside devices, mostly passives, 0603 and up. Does anyone have any experience with this? What are the pros/cons? What are the stencil design considerations? What about blades, material, angle, etc.? I have read that the standard stencil is thick plastic, but that better success is being achieved with laminated stainless. Does anyone have any experience with either? Any help is appreciated.

reply »

#19487

Screenprinting Adhesives | 12 April, 2002

We use steel stencils. The adhesive manufacturer can give recommendations for squeegee type, material, pressure, etc. A lot of the tech data sheets include this information.

reply »

Fuji Spares

#19490

Screenprinting Adhesives | 12 April, 2002

Screening adhesive can be messy but is alot quicker than using a glue machine as long as you setupyour stencil machine either manual or machine, we also use steel stencils with a stainless squeegee but you can use a rubber squeegee not sure about pressure/angle on a mchine printer as we use manual screen printer which you can adjust accordingly to get the best results - make sure you clean your stencils well at the end of the day espesially if you are printing 0603 as the holes are alot smaller - does this info help at all?

you can visit my site at http://www.fujispares.co.uk

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#19497

Screenprinting Adhesives | 12 April, 2002

Search the fine SMTnet Archives for background

reply »

Manufacturing Software

Reflow Ovens thermal process improvement