Dear all:

For PBGA replacement by a hot air BGA rework station, do I have to follow the same temperature profile as the first original one in the reflow oven? Note that in the rework process I use only Flux paste (no solder paste is used).

Hany

reply »

#18587

PBGA Rework Temperature Profile | 7 January, 2002

Your PBGA rework temperature profile should be similar to the same temperature profile as the first original one in the reflow oven. Searching the fine SMTnet Archives gives almost 500 postings on BGA and rework*.