You give no clue of what you want to write about. Let's try this:

J-STD-001, 8.3.1 Particulate Matter says words to the effect of solder balls / splats shall be neither: * Loose or able to be dislodged during normal service � NOR * Violate minimum electrical clearance.

A-610, 6.5.3.1 Excess Solder � Solder Balls / Splashes expands on the guidance of J-001, according to equipment classes.

You can purchase these documents through IPC [http://www.ipc.org]