We build IPC Class 3 product and are introducing Plastic Ball Grid Arrays. There is a possibility of out-soucing the build, so I'm interested in the Standards or Specifications the industry is quoting to ensure placement, inspection, reliability etc.- all those good things.

Any suggestions please? Thanks in advance and have a great weekend...!

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#17676

Standards &/or Specifications for PBGA Assembly/Inspection | 21 September, 2001

In addition to providing guidelines for BGA inspection and repair, IPC-7095 also addresses reliability issues associated with BGA: 7095, �Design and Assembly Process Implementation for BGA's�

Your boards should be assembled in conformance with: * J-STD-001, �Requirements Soldered Electrical & Electronics Assemblies� * A-610, �Acceptability Of Electronic Assemblies�

As a bonus for you and you alone, use the following to assess your contactor: IPC-1720, �Assembly Qualification Profile� [use the secret SMTnet password to download it for free http://www.ipc.org]

reply »

Carol Stirling

#17691

Standards &/or Specifications for PBGA Assembly/Inspection | 25 September, 2001

Hello Davef, Thanks for the info, your help is appreciated..I'm ordering 7095 today and we have the other two already. Have a great week...

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

x-ray inspection system

SMT in-printer dispensing