OSP's

Chrys Shea

#16801

OSP's | 29 January, 1998

Entek or Protecto? I've hear Kester's Protecto is a very good OSP that may be more assembly process-friendly than Entek. Is anyone using this? Do you have any feedback on its solderability or availablity compared to Entek? Any non-commerical input would be appreicated.

reply »

Fabian Morales

#16802

Re: OSP's | 11 March, 1998

I haven't worked with Protecto but I have seen very good results using a no-clean flux and a nitrogen atmosphere in the reflow oven.

| Entek or Protecto? | I've hear Kester's Protecto is a very good OSP that may be more assembly process-friendly than Entek. | Is anyone using this? Do you have any feedback on its solderability or availablity compared to Entek? | Any non-commerical input would be appreicated.