Dross limiting solutions | 19 February, 1998

Can anyone tell me any posible ways to help cut down on solder dross in an inert environment wave???? Any suggestions would be helpful.

reply »

Chrys Shea

#16702

Re: Dross limiting solutions | 20 February, 1998

| Can anyone tell me any posible ways to help cut down on solder dross in an inert environment wave???? Any suggestions would be helpful. It depends on how the environment is inerted. Is it a hood, tunnel, or boundary (Electrovert Contour) system? Does it have a hot gas knife for debrdging?