Flip chips - need info on handling and packaging

Diane Rogers

#15410

Flip chips - need info on handling and packaging | 16 June, 1998

Does anyone have experience working with flip chips? I would like to know how to work with them, some precautions, inspection techniques, etc. Thanks! Diane...

reply »

Russ Miculich

#15411

Re: Flip chips - need info on handling and packaging | 29 June, 1998

Diane: I would suggest you contact Chip Supply in Florida and find out how and what they specify to their suppliers. They inspect, test, package, and distribute many suppliers chips for flip chip and other applications. I am sorry but I do not have their address handy. Another supplier is Semi-Dice in Orange County, CA if you don't like the weather in Florida. Again, sorry, but I don't have the addresses handy. | Does anyone have experience working with flip chips? I would like to know how to work with them, some precautions, inspection techniques, etc. | Thanks! | Diane...