Selective Soldering | 14 September, 1998

Gentlemen, Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. Thanks in advance. George Henning

reply »

Rob Fischer

#14255

Re: Selective Soldering | 14 September, 1998

Have you considered using a masking wave solder pallet as opposed to going with new equipment. Utilizing Gerber files we have succesfully designed and manufactured this type of pallet for over five years. If this approach sounds like something you'd be interested in contact me at 215-340-0650 x 212; EMC Global Technologies. | Gentlemen, | Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? | My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. | Thanks in advance. | George Henning

reply »

Wayne Bracy

#14254

Re: Selective Soldering | 15 September, 1998

| Gentlemen, | Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? | My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. | Thanks in advance. | George Henning George: You might want to check out Exselect soldering Systems. Speak to Bill Sund sure he can give you loads of information of selected soldering and soldering systems. www.exselect.com

reply »

Chrys

#14253

Re: Selective Soldering | 15 September, 1998

| Gentlemen, | Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? | My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. | Thanks in advance. | George Henning George, I have been doing selective soldering with shielded pallets for eight years. They work really well, unless the board has very tall components (over 8 mm like aluminum electrolyitc caps) and do not suck up capital like selective soldering systems do. If pallets are not an option, Pillarhouse makes some nice systems. I've never used them, but I've checked them out at the trade shows and they seem pretty slick. Their number is (847) 593-9080.

reply »

Scott McKee

#14252

Re: Selective Soldering | 15 September, 1998

| Gentlemen, | Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? | My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. | Thanks in advance. | George Henning Try Air-Vac @ (203)888-9900 - East Coast (760)438-9363 - West Coast Good luck, Scott

reply »

Robert Murphy

#14251

Re: Selective Soldering | 17 September, 1998

| Gentlemen, | Can anyone provide information on selective soldering systems that compete with Ersa's VersaFlow? Does anyone have experience with this machine or other machines of this nature? | My company is considering acquiring to increase technical capability with double-sided mixed. We are wondering if this is the answer. | Thanks in advance. | George Henning George, If you might be interested in multi-wave selective soldering check out the New Age Electronic Devices web page at http://www.naed.com. I can also send you a copy of a paper on multi-wave selective soldering that I recently presented at a conference in Huntsville. If you would like a copy of the paper, either contact me by e-mail, and specify whether your e-mail software will accept attachments in Microsoft Word 6, or call me at (407) 847 - 7794.

reply »