Azote Soldering

Greg Flynn

#13767

Azote Soldering | 19 October, 1998

Has anybody out there, heard of a process/technology called AZOTE SOLDERING ???

reply »

Graham Naisbitt

#13768

Re: Azote Soldering | 19 October, 1998

Greg,

I may be mistaken but am fairly sure it means Nitrogen or inert gas soldering.

Soudage sous azote is French for Nitrogen soldering.

Hope this helps

Regards, Graham

Graham.Naisbitt@concoat.co.uk | Has anybody out there, heard of a process/technology called AZOTE SOLDERING ??? |

reply »

Greg Flynn

#13769

Re: Azote Soldering | 19 October, 1998

| Greg, | | I may be mistaken but am fairly sure it means Nitrogen or inert gas soldering. | | Soudage sous azote is French for Nitrogen soldering. | | Hope this helps | | Regards, Graham | | Graham.Naisbitt@concoat.co.uk | | Has anybody out there, heard of a process/technology called AZOTE SOLDERING ??? | | | Many Thanks Graham,

I was doing some Internet searching on the above topic and I was getting returns for French sites with descriptions like you have given. Sounds correct to me.

Thanks again, Greg |