Solder Paste Thinning | 27 October, 1998

Has anyone found a way to control viscosity of no-clean paste?

reply »

Dave F

#13672

Re: Solder Paste Thinning | 28 October, 1998

| Has anyone found a way to control viscosity of no-clean paste? | Mike: Mix it well and use the stuff before viscosity becomes an issue. Dave F