Chrys

#13114

Conductive Adhesives | 5 January, 1999

I'm looking for information on a company called AI Technologies. They make conductive adhesives and thermal management materials for attaching dice and heatsinks. Any feedback from users would be appreciated. Thanks,

Chrys

reply »

Dave F

#13115

Re: Conductive Adhesives | 5 January, 1999

| I'm looking for information on a company called AI Technologies. They make conductive adhesives and thermal management materials for attaching dice and heatsinks. Any feedback from users would be appreciated. Thanks, | | Chrys | Hey Chrys: I know that there was a recent thread on AI Tech on Technet recently. TTYL Dave F

A. I. Technology, Inc. P.O. Box 3081 Princeton, NJ 08543 USA Phone: (609)896-3838 Fax: (609)896-3315

reply »

Dave des

#13116

Re: Conductive Adhesives | 5 January, 1999

|Hi Chrys, any Tab tooling needs just call. Nice to talk tto you today, NEPCON is a maybe. Say Hi to Carlos.. Dave

I'm looking for information on a company called AI Technologies. They make conductive adhesives and thermal management materials for attaching dice and heatsinks. Any feedback from users would be appreciated. Thanks, | | Chrys |

reply »

Chrys

#13117

Re: Conductive Adhesives | 6 January, 1999

| | I'm looking for information on a company called AI Technologies. They make conductive adhesives and thermal management materials for attaching dice and heatsinks. Any feedback from users would be appreciated. Thanks, | | | | Chrys | | | Hey Chrys: I know that there was a recent thread on AI Tech on Technet recently. TTYL Dave F | | A. I. Technology, Inc. | P.O. Box 3081 | Princeton, NJ 08543 | USA | Phone: (609)896-3838 | Fax: (609)896-3315 | | Thanks, Dave. I went to the technet and searched the last three years' archives, but coulen't find anything specific to AI Tech.

Boy, when you go to another forum, you sure realize how much you appreciate the SMTNet, huh?

reply »

Dave F

#13118

Re: Conductive Adhesives | 6 January, 1999

| | | I'm looking for information on a company called AI Technologies. They make conductive adhesives and thermal management materials for attaching dice and heatsinks. Any feedback from users would be appreciated. Thanks, | | | | | | Chrys | | | | | Hey Chrys: I know that there was a recent thread on AI Tech on Technet recently. TTYL Dave F | | | | A. I. Technology, Inc. | | P.O. Box 3081 | | Princeton, NJ 08543 | | USA | | Phone: (609)896-3838 | | Fax: (609)896-3315 | | | | | Thanks, Dave. I went to the technet and searched the last three years' archives, but coulen't find anything specific to AI Tech. | | Boy, when you go to another forum, you sure realize how much you appreciate the SMTNet, huh? | Chrys: Now that you mention it, I don't believe that AI Tech was mentioned in the title of the tread, so your search would be futile, as you found. Where as on SMTnet, our search works in the message and you would have been able to find the thread. I'll poke around and try to find it over there.