I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help

reply »

Chris G.

#13041

Re: Selective Soldering | 10 January, 1999

| I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help | Jim,

Below are a couple of solder pot vendors I have used. You mention Air Vac. They make a PCBRM 10 or PCBRM12 and may have other models as well. They also make a complete selective soldering system including fluxer and preheat.

Hope this helps,

Chris

Air-Vac Engineering Company Inc. 30 Progress Avenue Seymour, CT 06483 Phone: (203) 888-9900 Fax: (203) 888-1145

Wenesco Inc. Box 59303 Chicago, IL 60659 Phone: (312) 973-4430 Fax: (312) 973-5104

reply »

Jason Nipper

#13042

Re: Selective Soldering | 12 January, 1999

| | I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help | | | Jim, | | Below are a couple of solder pot vendors I have used. You mention Air Vac. They make a PCBRM 10 or PCBRM12 and may have other models as well. They also make a complete selective soldering system including fluxer and preheat. | | Hope this helps, | | Chris | | Air-Vac Engineering Company Inc. | 30 Progress Avenue | Seymour, CT 06483 | Phone: (203) 888-9900 | Fax: (203) 888-1145 | | Wenesco Inc. | Box 59303 | Chicago, IL 60659 | Phone: (312) 973-4430 | Fax: (312) 973-5104 |

Hi Jim,

How's the weather up in Delavin? Here's a list of Vendors I have checked out. If you need any feedback on what I found, call me or email me.

Apollo Seiko Schiffer GmbH Corp. 4718 S. Pulaski Rd. Chicago, Il. 60632-4114 Ph (773) 847-2400 Fax (773) 847-5107

Automation Unlimited Inc, MRSI Corp 1640 Spruce St. Grafton, WI. 53024 Ph/Fax (414) 376-9427

Ersa N19W6721 Commerce Court Cederburg, WI. 53012 Ph (414) 375-6844 fax (414) 375-6849

Global Automation, Inc. 6 Vista Dr. Old Lyme, CT. 06371-1539 Ph (860) 434-6224 fax (860) 434-5448

Panasonic PFA 9377 W. Grand Ave. Franklin Park, IL. 60131 Ph (847) 288-4552 fax (847) 288-4564

JD Noble & Associates MTI Reena (847) 639-2440

reply »

Dick Casagrande

#13043

Re: Selective Soldering | 12 January, 1999

| | | I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help | | | | | Jim, | | | | Below are a couple of solder pot vendors I have used. You mention Air Vac. They make a PCBRM 10 or PCBRM12 and may have other models as well. They also make a complete selective soldering system including fluxer and preheat. | | | | Hope this helps, | | | | Chris | | | | Air-Vac Engineering Company Inc. | | 30 Progress Avenue | | Seymour, CT 06483 | | Phone: (203) 888-9900 | | Fax: (203) 888-1145 | | | | Wenesco Inc. | | Box 59303 | | Chicago, IL 60659 | | Phone: (312) 973-4430 | | Fax: (312) 973-5104 | | | | Hi Jim, | | How's the weather up in Delavin? Here's a list of Vendors I have checked out. If you need any feedback on what I found, call me or email me. | | Apollo Seiko | Schiffer GmbH Corp. | 4718 S. Pulaski Rd. | Chicago, Il. 60632-4114 | Ph (773) 847-2400 | Fax (773) 847-5107 | | | Automation Unlimited Inc, MRSI Corp | 1640 Spruce St. | Grafton, WI. 53024 | Ph/Fax (414) 376-9427 | | Ersa | N19W6721 Commerce Court | Cederburg, WI. 53012 | Ph (414) 375-6844 | fax (414) 375-6849 | | Global Automation, Inc. | 6 Vista Dr. | Old Lyme, CT. 06371-1539 | Ph (860) 434-6224 | fax (860) 434-5448 | | Panasonic PFA | 9377 W. Grand Ave. | Franklin Park, IL. 60131 | Ph (847) 288-4552 | fax (847) 288-4564 | | JD Noble & Associates MTI | Reena | (847) 639-2440 | |

Jim

One more for the list. Don't know anything about them.

New Age Electronic Devices 212 South Clyde Ave. Kissimmee FL 34741 407 847-7794 Email: rmurphy@iag.net http:/www.naed.com |

reply »

Chris G.

#13044

Re: Selective Soldering | 13 January, 1999

| I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help | Another for your list.

General Production Devices 2322 I-70 Frontage Road Grand Junction, CO 81505 1-800-742-5473

reply »