Conductive Adhesives and Underfill used on flex ckt | 11 January, 1999

I have used conductive adhesives for some time now on thickfilm. Does anyone know of a really good conductive adhesive to attach flip chips to flex circuits? I would like to stencil print the adhesive to the substrate and then place the flips chips onto the flex ckt substrate.

I also need a good flip chip underfill that will stick to to the Kapton flex material.

Thanks,

Chris

reply »

Earl Moon

#13015

Re: Conductive Adhesives and Underfill used on flex ckt | 12 January, 1999

| I have used conductive adhesives for some time now on thickfilm. Does anyone know of a really good conductive adhesive to attach flip chips to flex circuits? I would like to stencil print the adhesive to the substrate and then place the flips chips onto the flex ckt substrate. | | I also need a good flip chip underfill that will stick to to the Kapton flex material. | | Thanks, | | Chris | Interesting question as I need the same thing. I'm just starting to look at the problem I'll bet bit Jon Medernach has the answers to as I have always had problems with epoxy and Kapton.

Earl Moon

reply »

Earl Moon

#13016

Re: Conductive Adhesives and Underfill used on flex ckt | 12 January, 1999

| I have used conductive adhesives for some time now on thickfilm. Does anyone know of a really good conductive adhesive to attach flip chips to flex circuits? I would like to stencil print the adhesive to the substrate and then place the flips chips onto the flex ckt substrate. | | I also need a good flip chip underfill that will stick to to the Kapton flex material. | | Thanks, | | Chris | I did forget to mention the fine folks at Tessera as they nearly invented Micro-BGA. Vern Solberg and Joe Felstad are the gurus.