Beam lead attach

Kiet Dang

#8911

Beam lead attach | 19 October, 1999

I'm trying to set up a SPC for a thermo compression beam lead attach process. We're using a west bonder thermo compression machine. I'd appreciate any input on temperature, pressure,tool, and critical process considerations. thanks, -kiet.