Guys I'm looking for a software on the web that I can use to do void measurements. I have x-ray images but unfortunately no software in the machine to be able to calculate void size.

Thanks in advance for your support.

reply »

#76321

Voiding measure | 9 September, 2016

yoru x-ray supplier should be able to help however you can do a rough cut calculation byt just printing it out and measuring it, your interested in ration (%) of the void and where in the joint it is to tell you it it's really an issue. Also important to consider the use of the part, for example if it's high frequency then you actually don't really care about the void at all.