Hi, I have problem with one of the BGA Top Cap Detached from the Solder Balis attached to the BGA. Advice /Suggest why the Top Cap Has come out. We produced 4150 Pieces & had similar problems with 5 Pieces. Thx in advance for all your suggestions.

Thanks, Nagesh

Attachments:

reply »

#75876

BGA Top Cap Detached after reflow Soldering | 12 June, 2016

I'd guess that the interconnect pads on the BGA have poor solderability. Confirm this with testing at an independent lab. Work with your supplier to resolve the issue.