ideal solder paste viscosity

Views: 1305

#73915

ideal solder paste viscosity | 14 May, 2015

i want to know what is the ideal viscosity of solder paste before printing. i have brookfield viscosity meter with Spiral Spindle.

reply »

#73917

ideal solder paste viscosity | 14 May, 2015

I am pretty sure that will vary on the paste manufacturer. Using different amount and composition of flux will give you some different viscosity. I evaluated different solder paste brands before and I can tell you that some of them are very runny compared to others. Try to ask manufacturer of the paste about the recommended value.

reply »

#73918

ideal solder paste viscosity | 14 May, 2015

in enclosed data sheet mentioned 230Pa.s with malcom viscosity meter i have brookfield viscocity meter

kindly suggest

reply »