Non-conductive epoxy discoloration | 26 February, 2015

Hi, has anyone experienced discoloration of cured non-conductive epoxy? It turned from white to deep red. The parts were returned from customer and we noticed the color change and wondered what could cause epoxy discoloration.Thank you!