We are running Double sided PCB with SMD components at Bottom through Wave solder. So we are using selective carrier for PCBs with pouch just for this RJ45 1X4 Connector. We run PCBs with "connector perpendicular to wave" _______ _______ ------> Travel Direction

Similar Part : http://nz.rs-online.com/web/p/rj45-connectors/8208205/

And we are getting Solder short on every PCB and also additionally Dry joints (leads) on some. Played with Flux adjustments and also Parameter settings for wave, but still same. Suggest me if there is any solution for getting this connectors properly soldered with no issue.

Thanks.

reply »

#73543

RJ45 1X4 Way Connector | 17 February, 2015

What kind of flux are using? What is your conveyor speed? What is the solder pot temp?

Thanks, George

reply »


VB

#73629

RJ45 1X4 Way Connector | 3 March, 2015

Hi

Kester 979. (No clean flux) Solder pot temp - 280 Conveyor speed - tried (1-2M) but same

Thanks