Solder Bridging On SMD Pad for Nexlev Connector

Views: 2679

#72979

Solder Bridging On SMD Pad for Nexlev Connector | 29 October, 2014

Help Needed.

I face a solder bridging issue on solder mask define pad at edge only for nexlev connector . The pad design such as smd at four corner only. The bridging happen on signal to ground pin only. Current stencil we use 22 round with 6 mils step up for stencil and at the edge we use 20 round with 6 mils step up. So far we already check printing , pick and place and profile as well but don't why the bridging happen at edge on nexlev connector smd only. please help me ...

reply »

#72986

Solder Bridging On SMD Pad for Nexlev Connector | 30 October, 2014

What's the software you are using? Modify it manually. It should not be difficult.