High Melting point Solder wire

Views: 867

#72107

High Melting point Solder wire | 13 May, 2014

I am looking for the solder wire leaded or lead free which can withstand the solder joint at temperature 450deree Celsius or more after soldering, since i need to form a solder joint at higher temperature area Pls suggest the part number for the same

reply »

#72108

High Melting point Solder wire | 13 May, 2014

There are many alloys of silver solder for higher temperatures mostly used in plumbing There are also alloys which are available in paste form used in the manufacture of hybrids.

sarason

reply »