Disposition on Discoloration of Boards post reflow | 26 December, 2013

Hi , During one of NPI trial ,we found that boards ( CEM -1 grade )has got discolored on the masking portion ( and not on the conductors) after reflow .Although it does not impact our Form /Fit and Function characteristics , I would like to get your opinion on the following : 1) What kind of disposition is to be taken ? should it be Go-No-Go ? 2) Is there any standard which gives reference to discoloration of boards disposition . I checked in 610 and it does not gives wrt to the board info. but it surely gives reference of conductors which is not our case study . Please advise . Regards Vikas

reply »

#71535

Disposition on Discoloration of Boards post reflow | 30 December, 2013

A-610E, 10.7.4 covers solder mask discoloration. Use that for your disposition

reply »

#71538

Disposition on Discoloration of Boards post reflow | 30 December, 2013

Hi Dave , Thanks and will align accordingly .

reply »