Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.

important parameters - wave soldering

Views: 1385


important parameters - wave soldering | 27 October, 2013

What are the parameters that are more important for perfect soldering and how are they defined.

reply »


important parameters - wave soldering | 28 October, 2013

Two most important parameters are: * Solder temperature is the temperature of the solder * Dwell time is the time that the board remains in contact with the molten solder

Several things that you should consider are: * First, here's how to design an experiment:

* Second, design pitfalls that can lead to solder shorts during wave solder:

* Third, a troubleshooting guide is always handy:

* Next, a good overview of process helps with context:

reply »

reflow oven profiler

Metcal soldering rework