Required magnifier for inspection of 0603 component

Views: 1413

#71152

Required magnifier for inspection of 0603 component | 28 September, 2013

Hi Everyone,

What is required magnification to inspect 0603 component?

ernie

reply »

#71169

Required magnifier for inspection of 0603 component | 30 September, 2013

Hi, Ernie,

According to IPC610, for land widths > 1 mm, recommended inspection range is from 1.5X to 3X magnification. For verification of rejects, 4X magnification is recommended.

Cheers, ..rob