Solder Ball Composition | 25 April, 2013

Hi, I have a BGA ball with composition 98.3Sn 1Ag 0.7Cu Does anyone know what is the effect if I increase or decrease the amount of Sn, Ag, or Cu? And what if I add Ni inside? Can anyone explain to me? Many thanks in advance.

reply »

#68743

Solder Ball Composition | 25 April, 2013

Hi,

I attach two pictures for you. Hope they help

Attachments:

reply »

#68745

Solder Ball Composition | 25 April, 2013

Hi, thanks for the pictures. May I know in the first picture what are those numbers (i.e. 280, 290, 300, 310, etc) represent?

reply »

#68748

Solder Ball Composition | 26 April, 2013

These numbers show liquidus temperature in C for each alloy combination.