Does anyone know of a masking material that could be applied over test pads that could be left on board that ICT test probes will pierce? could be tape or dispensed material.

Thanks!!

reply »

#68193

Choices ... You got choices | 13 February, 2013

Things that come mind are: * Not sure why you want to do this, since probing solder gives a longer probe life than probing copper. * I've never tried it, but I see no reason why you couldn't probe Kapt0n or blue painters tape. * Fabs [or you] can print temporary solder mask.