Pin In Hole Size

gregH

#6920

Pin In Hole Size | 18 June, 2001

I have a 10-pin single in line connector that is reflowable. Pin size is 1.0mm and my pcb drill size diameter for the pin is 1.5mm. is it okay for pin in hole process ? I have only 2 pcs of pth components and they are the 2 10 SIL connectors. What's a good ratio of pth versus lead diameter for a good Pin in hole process ?

thanks

reply »

#6963

Pin In Hole Size | 18 June, 2001

Sounds good to me. Check the references on "Pin & Paste on Thick PCBs" June 15, 2001 09:13 AM