PCB contamination with NC Flux after Wave Solder | 22 October, 2012

We use a NC Flux in the wave solder and after aAcelerated Life Test cicle we found contamination white residues paths between some solder points. Does somebody know a possible cause for this contamination.

Attachments:

reply »

#67559

PCB contamination with NC Flux after Wave Solder | 23 October, 2012

Ideally first you need to analyze the residue to see what it is. We had a customer with white residues after wave and elemental analysis revealed tin.

reply »

#67560

PCB contamination with NC Flux after Wave Solder | 23 October, 2012

thank you for the information .We are planning to send the units for analysis.