Glue parts coming off | 29 June, 2012

We are having some problems with parts that are glued on untill our PCBs go to wave coming off. We would like to test the stenght of the glue. Does anyone have any ideas on how to test pull off strength, torque strength, and push off strength? Any information would be helpful!

reply »

#66715

Glue parts coming off | 29 June, 2012

Here's a link to one of my favorite threads on measuring glue from the fine SMTnet Archives ... http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=17437