Blue-Film on surface of leadfree Pot | 30 May, 2012

Recently we have noticed a purple-blue colour film on the surface of the molten solder. It can be cleared when de-drossing the pot. The pot will normally go a yellow/gold colour before it turns purple-blue. Is this most likely an oxide of the tin or is this a contamination issue?

Attachments:

reply »

#66466

Blue-Film on surface of leadfree Pot | 31 May, 2012

This is common and not an issue it is just the surface oxide

Bob Willis

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#66469

Blue-Film on surface of leadfree Pot | 31 May, 2012

Thanks Bob