Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Tin-Bismuth Eutectic

Views: 4469

#65621

Tin-Bismuth Eutectic | 10 December, 2011

Dear Friends, I would like to know whether any of you evaluating with Low Temperature Solder especially Tin-Bismuth-Silver COmbination. If you have any feedback/articles/evaluation/reliability/Yield Reports, please share.

Regards Vijai

reply »

#65641

Tin-Bismuth Eutectic | 13 December, 2011

Here is a link to an interesting Ron Lasky blog posting on the topic http://blogs.indium.com/blog/an-interview-with-the-professor/has-the-time-come-for-tin-bismuth-solders

We have no relationship, nor receive benefit from the company referenced above.  

reply »


aci

#65647

Tin-Bismuth Eutectic | 14 December, 2011

We currenty process SnBi. I have not ever seen silver added though. What kind of issues are you having?

reply »

#65651

Tin-Bismuth Eutectic | 14 December, 2011

Hi Dave, Thanks for sharing

reply »

#65652

Tin-Bismuth Eutectic | 14 December, 2011

Hi, I didnt use currently . . . but seriously looking to make use of SnBi or SnBiAg. I would like to know any limitations/reliability study on this process . . . moreover need some guidance/help to adopt this alloy in process

Regards Vijai