What does OA stand for?

Spanky

#6667

What does OA stand for? | 23 May, 2001

I know that OA is water soluable. But what exactly does the acronym "OA" stand for? "Organic something-or-other". I've checked the archive and can only find reference to oa, not what it actually stands for.

thanks, spanky

reply »


K

#6670

What does OA stand for? | 23 May, 2001

I beleive it's Organic Acid

reply »

Paul Christiansen

#6715

What does OA stand for? | 29 May, 2001

I will second the previous answer that it stands for Organic Acid. "Acid" being the key word as to why it must be thoroughly cleaned.

reply »

Robert Sykoh

#6720

What does OA stand for? | 29 May, 2001

OA stands for Organic Activated. In the good old fo SMT processes, a lot of different fluxes are being considered. RA, RMA, OA, etc. If you look at the present no-clean paste, it is actually RMA.