Hi,

what kind of issues i could get if the i do not provide heal properly in my footprint ?

In my current design 0603 resistor package footprint heal is missing by 3 mils each side

Please help

reply »

#64719

SMT Heal Issue | 28 July, 2011

The consequences of poor heel formation in solder connections include: * Lower solder joint strength * Possible intermittent short circuits * Reduced first-pass yields * Increased inspection cost * Increased rework cost * Likely field failures * Likely damage to your company's brand & image * Likely educed sales and profits