solder paste release from stencil | 19 July, 2011

Has anyone tried using a product thet when applied to a stencil, it facilitates the release of solder paste from the stencil, including the fine pitch openings. It makes the stencil's surface "fluxophobic". Same principle as Rain-X for windshield.

Anyone?

reply »


Ken

#64672

solder paste release from stencil | 20 July, 2011

I think you are referring to nano coatings. Try google nano coated stencils

reply »

#64675

solder paste release from stencil | 20 July, 2011

I just asked the same question a few weeks ago. Here's the link to that thread: