Has anyone done any testing with UV tracer in Parylene processing? Does it cause adhesion problems? Does anyone have any data they can share on this.

reply »


Lou

#64598

UV Tracer in Parylene | 6 July, 2011

We do parylene coating and really frown upon using a UV additive. Technically, it's a contaminant to the parylene.

reply »

#64605

UV Tracer in Parylene | 7 July, 2011

I had read somewhere that parylene absorbs UV radiation, and therefore offers very low UV protection. So, yeah probably not a good idea. Plus since it's vapor deposited, unless there is no access to a surface, all surfaces are covered.

reply »

#64633

UV Tracer in Parylene | 11 July, 2011

Lou, Oh really? Why's that?