Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Flux mixed with Thinner

Views: 3703

#64232

Flux mixed with Thinner | 28 April, 2011

Hi All I received some advice 1) use Flux with Thinner 2) use Flux with Water. Which one is better for my wave sodlering? The type of Flux is watersoluble.

reply »

#64233

Flux mixed with Thinner | 28 April, 2011

We'd guess thinner, but more importantly, what does the formulator of your flux say?

reply »


aci

#64234

Flux mixed with Thinner | 28 April, 2011

You should only need to mix in thinner if your formulation changes. You will need to check the specific gravity of your flux. You can do this by using a hydrometer. Contact your flux supplier for their advice.

reply »

#64237

Flux mixed with Thinner | 28 April, 2011

Dear Dave

Thanks for your advice.I dun know why flux can't use alone w/o adding other solvents. is it neccessary? Now, our flux density is 0.88. By the way, we use Hi Grade Flux 1080.

reply »

#64279

Flux mixed with Thinner | 6 May, 2011

use thinner and contact your supplier about it. the guy that advised you to use water is probably from your competitor. LOL