I need 15 - 25 microns (T5) Solder Paste

Views: 3126

#63428

I need 15 - 25 microns (T5) Solder Paste | 5 January, 2011

I am looking for a No-clean or water soluble solder paste, Sn63/Pb37 alloy, 15 - 25 microns (T5). I need to print with a 4.8 mil stencil opening. Does anyone know where I can get 250 to 500 grams in one week or less?

reply »

#63429

I need 15 - 25 microns (T5) Solder Paste | 5 January, 2011

Where you are? http://www.esdcoats.net pls check if we are near from you.

reply »

#63438

I need 15 - 25 microns (T5) Solder Paste | 6 January, 2011

Indium has it.