Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Has anyone else had failures with Leds made by EOI

Views: 1884


MM

#63129

Has anyone else had failures with Leds made by EOI | 15 November, 2010

Has anyone else had failures with Leds from EOI? The part number is EOZ-ZARNCD0-DG. We are using a lead free no clean process using SAC305 solder. These are thru hole parts and our max temp is 244 for 3 seconds. Please if anyone else had issues or has issues, please let me know. Thanks for any input.

reply »

#63131

Has anyone else had failures with Leds made by EOI | 15 November, 2010

Hi. Michelle. What kind of problem do you want to know? Soldering issue?

Thanks Ju

reply »

#63133

Has anyone else had failures with Leds made by EOI | 15 November, 2010

Hi. Michelle. What kind of problem do you want to know? Soldering issue?