Dear All Does anyone know about the low melting point solder paste which should be Copper Base? Usually the Copper base solder has 227'C of melting point.

reply »

#63024

looking low melting solder paste | 31 October, 2010

#63029

looking low melting solder paste | 1 November, 2010

Hi Mark thanks and useful. However, I couldn't find the Copper base solder paste which melting point is lower than 210'C.

reply »

#63031

looking low melting solder paste | 1 November, 2010

Jacki,

Lead-free Cu based alloys with melting point below 210C don’t exist.

reply »

#63035

looking low melting solder paste | 2 November, 2010

Hi Patrick Noted that. Thanks for ur info.